I-Hastelloy C2000 8.0*1.25 mm ishubhu elihlanganisiwe

Incazelo emfushane:

Ukwakheka Kwamakhemikhali

I-Hastelloy C2000 8.0*1.25 mm ishubhu elihlanganisiwe

Ukwakheka kwamakhemikhali e-Hastelloy C-2000 kukhonjisiwe etafuleni elingezansi:

Isici Ubuncane % Ubuningi %
Cr 22.00 24.00
Mo 15.00 17.00
Fe - 3.00
C - 0.01
Si - 0.08
Co - 2.00
Mn - 0.50
P - 0.025
S - 0.01
Cu 1.30 1.90
Al - 0.50
Ni bal

Ingxubevange Imininingwane

Ukuminyana kwe-Hastelloy C-2000, indawo encibilikayo, i-coefficient yokunwetshwa, kanye nemodulus yokunwebeka kukhonjisiwe kuthebula elingezansi:

Ukuminyana I-Melting Point I-Coefficient of Expansion I-Modulus of Rigidity I-Modulus ye-Elasticity
8.5 g/cm³ 1399 °C 12.4 μm/m °C (20 – 100 °C) 79 kN/mm² 206 kN/mm²
0.307 lb/in³ 2550 °F 6.9 x 10-6ku-°F (70 – 212 °F) 11458 k 29878 nxa
 

Ukwelashwa kokushisa kwezingxenye eziqediwe

I-Hastelloy C2000 8.0*1.25 mm ishubhu elihlanganisiwe

Ukwelashwa okujwayelekile kokushisa kwe-Hastelloy C-2000:

Umbandela njengoba uhlinzekwe yi-AWI Uhlobo Izinga lokushisa Isikhathi Ukupholisa
I-Annealed noma i-Spring Temper Yehlisa Ingcindezi 400 – 450 °C (750 – 840 °F) 2 Hr Umoya
I-Hastelloy C2000 8.0*1.25 mm ishubhu elihlanganisiwe

Izakhiwo

Izakhiwo ezijwayelekile zemishini ye-Hastelloy C-2000:

I-Annealed    
Cishe.amandla aqinile <1000 N/mm² <145 ksi
Cishe.izinga lokushisa lokusebenza kuye ngomthwalo ** kanye nendawo -200 kuya +400 °C -330 kuya +750 °F
I-Hastelloy C2000 8.0*1.25 mm ishubhu elihlanganisiwe
I-Spring Temper    
Cishe.amandla aqinile 1300 - 1600 N/mm² 189 – 232 ksi
Cishe.izinga lokushisa lokusebenza kuye ngomthwalo ** kanye nendawo -200 kuya +400 °C -330 kuya +750 °F

Imininingwane Yomkhiqizo

Omaka bomkhiqizo

Ukwakheka Kwamakhemikhali

I-Hastelloy C2000 8.0*1.25 mm ishubhu elihlanganisiwe

Ukwakheka kwamakhemikhali e-Hastelloy C-2000 kukhonjisiwe etafuleni elingezansi:

Isici Ubuncane % Ubuningi %
Cr 22.00 24.00
Mo 15.00 17.00
Fe - 3.00
C - 0.01
Si - 0.08
Co - 2.00
Mn - 0.50
P - 0.025
S - 0.01
Cu 1.30 1.90
Al - 0.50
Ni bal

Ingxubevange Imininingwane

Ukuminyana kwe-Hastelloy C-2000, indawo encibilikayo, i-coefficient yokunwetshwa, kanye nemodulus yokunwebeka kukhonjisiwe kuthebula elingezansi:

Ukuminyana I-Melting Point I-Coefficient of Expansion I-Modulus of Rigidity I-Modulus ye-Elasticity
8.5 g/cm³ 1399 °C 12.4 μm/m °C (20 – 100 °C) 79 kN/mm² 206 kN/mm²
0.307 lb/in³ 2550 °F 6.9 x 10-6ku-°F (70 – 212 °F) 11458 k 29878 nxa

Ukwelashwa kokushisa kwezingxenye eziqediwe

I-Hastelloy C2000 8.0*1.25 mm ishubhu elihlanganisiwe

Ukwelashwa okujwayelekile kokushisa kwe-Hastelloy C-2000:

Umbandela njengoba uhlinzekwe yi-AWI Uhlobo Izinga lokushisa Isikhathi Ukupholisa
I-Annealed noma i-Spring Temper Yehlisa Ingcindezi 400 – 450 °C (750 – 840 °F) 2 Hr Umoya
I-Hastelloy C2000 8.0*1.25 mm ishubhu elihlanganisiwe

Izakhiwo

Izakhiwo ezijwayelekile zemishini ye-Hastelloy C-2000:

I-Annealed
Cishe.amandla aqinile <1000 N/mm² <145 ksi
Cishe.izinga lokushisa lokusebenza kuye ngomthwalo ** kanye nendawo -200 kuya +400 °C -330 kuya +750 °F
I-Hastelloy C2000 8.0*1.25 mm ishubhu elihlanganisiwe
I-Spring Temper
Cishe.amandla aqinile 1300 - 1600 N/mm² 189 – 232 ksi
Cishe.izinga lokushisa lokusebenza kuye ngomthwalo ** kanye nendawo -200 kuya +400 °C -330 kuya +750 °F