Siyakwamukela kumawebhusayithi ethu!

2205 insimbi engagqwali coiled tubing

I-SAF 2205 Duplex Stainless Steel

I-SAF 2205 insimbi engagqwali yakhiwe nge-22% chromium, 2.5% molybdenum, kanye ne-4.5% ye-nickel nitrogen alloy.Inamandla aphezulu, ukuqina komthelela omuhle, nokumelana nokucindezeleka okuhle.

2205 insimbi engagqwali coiled tubing

Amandla okukhiqiza e-SAF 2205 duplex steel stainless aphakeme ngokuphindwe kabili kunalawo ensimbi engenasici ye-austenitic evamile.Lesi sici singanciphisa isisindo sokusetshenziswa, okwenza le alloy ingabizi kakhulu kuno-316 no-317L.Le ngxubevange ifaneleka ngokukhethekile izinga lokushisa elingu-50 ° f / + 600 ° F.

2205 insimbi engagqwali coiled tubing

Le alloy ingacatshangelwa futhi ngezinhlelo zokusebenza ezingaphezu kwalolu banga lokushisa, kodwa kunemikhawulo ethile, ikakhulukazi uma isetshenziselwa izakhiwo ezishiselwe.

2205 insimbi engagqwali coiled tubing

2205 ukwakheka kwamakhemikhali ensimbi engagqwali

  C Mn Si P S Cr Ni
Ubukhulu 0.08 1.5 2.00 0.04 0.04 21.0 11.0
Okuncane - - - - - 18.0 8.0
2205 insimbi engagqwali coiled tubing

Izakhiwo Zemishini

Amandla esivuno (Rp0.2 / MPa) ≥227
Amandla okuqina (Rm / MPa) ≥973
Umthelela (Kv / J) 34
Ubude (A / %) 14
Ukuminyana 7.8 g/cm³
Ukuqina (HB) 242

Isicelo

2205 insimbi engagqwali coiled tubing

  • Umkhumbi wokucindezela, ithangi lokugcina umfutho ophezulu, ipayipi lomfutho ophezulu, isishintshi sokushisa
  • Ipayipi likawoyela negesi
  • Ukwelashwa kwendle
  • Imboni ye-Pulp kanye nephepha, imishini yokuxubha, ukugcinwa kanye nezinhlelo zokucubungula
  • I-Rotary shaft bese ucindezela u-roll ngamandla aphezulu kanye nendawo evikela ukugqwala
  • Ibhokisi lempahla lomkhumbi noma iloli
  • Imishini yokucubungula ukudla

Isikhathi sokuthumela: Jul-02-2023